» Sign in / Register

Alkyne Magnetic Beads

Cat. No. Amount Price (EUR) Buy / Note
CLK-1035-1 1 ml 218,40 Add to Basket/Quote Add to Notepad
Structural formula of Alkyne Magnetic Beads
Structural formula of Alkyne Magnetic Beads

For research use only!

Shipping: shipped at ambient temperature

Storage Conditions: store at 4 °C
do not freeze

Shelf Life: 12 months after date of delivery

Form: 10 mg/ml suspension containing 0.05 % Kathon

Applications:
Alkyne Magnetic Beads are an efficient magnetic matrix to covalently capture CLICK-functionalized proteins by a Cu(I)-catalyzed azide-alkyne cycloaddition (CuAAC). The proteins of interest need to be metabolically, enzymatically or chemically azide-tagged. Subsequently, the azide magnetic beads containing the covalently attached proteins can be washed with high stringency, virtually eliminating any non-specifically bound proteins.
Alkyne Magnetic Beads are not stable in organic solvents and high urea concentrations. Use Alkyne Agarose(CLK-1032) for mass spectrometry experiments.

Degree of substitution: 30-50 nmol Alkyne-groups/ mg resin
Surface area: 5.7 * 109 μm2/mg
Mean bead diameter: 0.97 μm
Density: 1.33 g/cm3
Polymere composition: benzene, ethyenyl- and homopolymer (encapsulated magnetite)